OFFICE MEMO MIL-I-46058C Coat. Adh. Coupons Date:6/15/95
We are implementing a low residue process and want to be sure the bags we use
do not introduce contamination that will affect our hardware or interfere
with conformal coat adhesion. I just reviewed a study in which 'Kapak' bags
were used in a similar situation.
I am looking for a source for MIL-I-46058C conformal coat adhesion test
coupons. Any information would be greatly appreciated.