TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipchq.com (Smail3.1.28.1 #2) id m0s8qJh-0000HZC; Tue, 9 May 95 09:31 CDT
Old-Return-Path:
<miso!smtplink.dsccc.com!geiland>
Date:
Mon, 08 May 95 13:45:31 CST
Precedence:
list
X-Loop:
From [log in to unmask] Thu Apr 25 15:
26:18 1996
Resent-Sender:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/477
TO:
Return-Path:
Resent-Message-ID:
<"dH5DF.0.DjB.kothl"@ipc>
Subject:
From:
"geiland" <[log in to unmask]>
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (38 lines)

According to the test report from Enthone-OMI, the DSR-3241 dielectric strength 
is greater than 500volts DC/mil.  For more information, you can contact Dave 
Stone at (203) 932-8631.

______________________________ Reply Separator _________________________________
Subject: Enthone DSR 3241 Solder Mask
Author:  BWOOLDRI at DSC-1100
Date:    5/8/95 9:19


Gary,

I got this over the IPC TechNet.  Maybe you can help her.

Bruce


______________________________ Forward Header __________________________________
Subject: Enthone DSR 3241 Solder Mask
Author:  [log in to unmask] at SMTPLINK 
Date:    05/04/95 04:09 PM


From: Kelly Kovalovsky, Raw Card Quality Engineering                           
_     Phone:704-595-7336 Tie Line:795-7336 FAX Ext. 4727                       
Subject: Enthone DSR 3241 Solder Mask                                          
Can someone provide me with the dielectric strength of Enthone DSR             
3241 solder mask?                                                              

Kelly Kovalovsky                                                               
IBM Microelectronics Division                                                  
6800 IBM Drive MG12/251                                                        
Charlotte, NC  28262-8563                                                      