TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
[log in to unmask][log in to unmask]>
To: MR DOUGLAS C JEFFERY <[log in to unmask]>
Cc: [log in to unmask]
Subject: Re: Tin/lead plating vs HAL [...]39_Pine.3.89.9506211229.E46751-0100000@ipc0_0_
Date:
Thu, 23 Nov 95 12:12:12 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
     
     Dear members,
     
     I am promoting mecseal finish for doubleside SMD jobs to our 
     customers.
     
     One customer pointed out the following problem.
     
     Two mounting holes(pth) is taped during wawesoldering and subsequently
     brackets are fixed.He needs to ground the bracket and nut should make
     electrical contact with land surrounding the fixingholes.Since the
     fixing holes are covered with tape and subsequently tape is removed
     meseal is not removed in that part.This will lead to no electrical 
     contact between the nut and the hole including land surrounding
     
     Any suggestion to over come this problem please.May be some design
     alternative to overcome this problem
     
     Since OSP enteck etc. are in existence for quitesometime I think
     someone might have this problem and overcome also.
     
     Thanks in advance for any response
     R.Srinivasan
     Engineering mgr