If you would like some information on the immersion gold process in terms of
reliability after ageing and the assembly yields you can get a copy of my colour
report on the subject, its FREE from Shipley. It was produced two years ago when
the use of the gold process was starting in Europe and many of our members were
ito the process.

You should contact:
Arthur Wolfrum
Tel: 508 481 7950
Fax: 508 229 0853

Bob Willis
VP SMART Group
European Surface Mount Association.
Tel: 01245 351502
Fax 01245 496123