Subject: | |
From: | |
Reply To: | Mickey Weiner (2937) |
Date: | Wed, 26 Jul 1995 08:30:53 +0300 (IDT) |
Content-Type: | TEXT/PLAIN |
Parts/Attachments: |
|
|
hi tom,
A reference which we keep using as a guide is found in mil-f-14072b,
para. 3.13 and the table of "compatible couples".
There are also solderability issues associated with gold plated lugs.
regards,
mickey
On Thu, 20 Jul 1995, Tom Tindale wrote:
> We have a customer who requires tin/tin type sockets as opposed to tin/gold
> for all their socketed components. Their reasoning is based on the corrosion
> potential from the dissimilar metals. Our problem is that tin/tin sockets
> are becoming increasingly more difficult to obtain, and in some cases more
> expensive than their gold plated counterparts. My question is: Has anyone
> have any information or done any testing on this subject. We would like to
> change their thinking if possible. Any information would be appreciated.
>
> Thanks,
>
> Thomas Tindale
> Lead Manufacturing Engineer
> Performance Computer
> 315 Science Parkway
> Rochester, New York 14620
> 716.256.0200 Phone
> 716.256.0791 Fax
> e-mail [log in to unmask]
>
|
|
|