	I am looking for any information concerning the minimum distance between
	a via to smt land (1206, 0805, and 0603). Currently we are using a 
        .015 hole / .030 pad non-tented via. Is anyone out there burying the
	via in the center of the land? The wave side is not as much of a concern
        as the reflow side. We are planning to run some test boards with several
	configurations. I would appreciate any feed back.


	Tom Vaillancourt
	Philips Consumer Electronics Co.
	615-521-3482
	Internet: [log in to unmask]