TECHNET Archives

1995

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipchq.com (Smail3.1.28.1 #2) id m0sK52h-0000HAC; Fri, 9 Jun 95 09:28 CDT
Old-Return-Path:
<miso!macmail1.cig.mot.com!Wrezel_Jim>
Date:
8 Jun 1995 21:11:52 -0500
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/581
TO:
"IPC 1" <[log in to unmask]>, "Leo Reynolds" <[log in to unmask]>
Return-Path:
Resent-Message-ID:
<"gnTFh.0.9w8.cf5sl"@ipc>
Subject:
From:
"Wrezel Jim" <[log in to unmask]>
Resent-Sender:
X-Loop:
X-Mailer:
Mail*Link SMTP/MS 3.0.0
From [log in to unmask] Sat Apr 27 14:
17:25 1996
Parts/Attachments:
text/plain (67 lines)
Leo,

We have observed this phenomenon on polycarbonate telephone housings, but not
on circuit boards.  The pink bags will emit antistatic compounds, especially
at elevated temperature and humidity.  FTIR or SIMS analysis can be used to
confirm the presence of the liberated antistat if it is on your boards. 
Amide, amine  and amine/ammonium salt compounds are used as antistats for
this application, although the majority of pink bags are formulated with
amides due to their relative chemical inertness.  However, one should
evaluate whether amines are present since insulation resistance could be
compromised.

Regards,
Jim Wrezel
Motorola, Inc. 
_______________________________________________________________________________
From: Leo Reynolds on Thu, Jun 8, 1995 5:34 PM
Subject: Pink Poly Bags/Shipping PCB Assy's
To: [log in to unmask]



Hello;

Our question is "Has anyone experienced a problem with shipping PCB 
Assys in pink poly bags and having contamination develop on the PCB from 
outgassing of the plastic bag.  The assys we've noted the problem with 
have typically been air shipped, at least some of them to the Orient."

Thank You in advance for any light you might be able to shed on this 
particular phenomenon.


Best Regards,


Leo


------------------ RFC822 Header Follows ------------------
Received: by macmail1.cig.mot.com with SMTP;8 Jun 1995 17:34:37 -0500
Received: from motgate.mot.com (motgate.mot.com [129.188.136.100]) by
pobox.mot.com (8.6.11/8.6.10/MOT-3.7) with ESMTP id RAA19570 for
<[log in to unmask]>; Thu, 8 Jun 1995 17:34:35 -0500
Received: from gagme.wwa.com (miso.wwa.com [198.49.174.33]) by
motgate.mot.com (8.6.11/8.6.10/MOT-3.7) with SMTP id RAA22241 for
<[log in to unmask]>; Thu, 8 Jun 1995 17:34:34 -0500
Resent-Date: Thu, 8 Jun 1995 17:34:34 -0500
Received: from ipc by gagme.wwa.com with uucp
	(Smail3.1.28.1 #8) id m0sJqEk-000FILC; Thu, 8 Jun 95 17:39 CDT
Received: by ipchq.com (Smail3.1.28.1 #2)
	id m0sJpZW-0000GoC; Thu, 8 Jun 95 16:57 CDT
Old-Return-Path: <miso!ix.netcom.com!LEOT1>
Date: Thu, 8 Jun 1995 14:05:39 -0700
Message-Id: <[log in to unmask]>
From: [log in to unmask] (Leo Reynolds)
Subject: Pink Poly Bags/Shipping PCB Assy's
To: [log in to unmask]
Resent-Message-ID: <"g1m-y2.0.94F.h8trl"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/580
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]



ATOM RSS1 RSS2