Received: |
by ipchq.com (Smail3.1.28.1 #2)
id m0sbB8y-0000GoC; Wed, 26 Jul 95 13:25 CDT |
Content-Type: |
TEXT/PLAIN; charset=US-ASCII |
Old-Return-Path: |
<bergda> |
Date: |
Wed, 26 Jul 1995 13:25:15 -0500 (CDT) |
Precedence: |
list |
From [log in to unmask] Sat Apr 27 14: |
25:51 1996 |
cc: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
|
X-Status: |
|
Resent-Sender: |
|
Resent-Message-ID: |
<"EsmZX1.0.-pE.EYe5m"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
In-Reply-To: |
|
Resent-From: |
|
Message-ID: |
<Pine.3.89.9507261308.E54855-0100000@ipc> |
Parts/Attachments: |
|
|
Rich, I would suggest looking at the aging requirments for boards in
J-STD-003 this was developed after extensive literature review and IPC
round robin testing. I would also suggest review of IPC-TR-464
Accelerated Aging for Solderability Evaluations, and IPC-TR-462,
Solderability Evaluation of Printed Boards with Protective Coatings Over
Long Term Storage.
Regards
***************************************************
David W. Bergman, Technical Director
IPC
7380 N. Lincoln Avenue
Lincolnwood, IL 60646
708-677-2850 x340 Phone
708-677-9570 Fax
email [log in to unmask]
***************************************************
On Tue, 25 Jul 1995 [log in to unmask] wrote:
> Hello,
>
> I would like to do some accelerated aging tests for solderability
> of eutectic solder. The solder is over nickel over copper on board
> material (FR-4). Does any one know any respectable tests in the
> literature that claim to approximate 6 months and 1 year of solder
> aging. If such a claim is not explicitly stated how are the results of
> such tests viewed. Does the I.P.C. recommend a particular test. How
> about the military? I have a programmable temperature and humidity
> chamber at my disposal , but would like information on all tests.
>
> Thanks
> Rich
> ------------------------------------------------------------------
> Richard Olsen Telephone (602)-268-3461
> Continental Circuits Corp. Fax (602)-268-0208
> 3502 East Roeser Road Pager (602)-310-6245
> Phoenix Arizona Internet [log in to unmask]
> 85040-2905
> USA I make circuit boards,what do you do?
> ------------------------------------------------------------------
>
>
|
|
|