Thanks very much everyone!
Potting materials are looking the most promising.
Just sent a request for info to Epic and hopefully you'll get some thanks from them Steve.
Richard Hatano
EDA Manager
3855 Ruffin Road, San Diego, CA 92123-1813 USA
Direct 858-285-2392 | Fax 858-836-3400
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, May 3, 2021 3:05 PM
To: [log in to unmask]
Subject: Re: [TN] [External] Re: [TN] TechNet archives? looking for information on coating or encapsulation long term protection
EXTERNAL SENDER – Exercise Caution.
We use some potting stuff from Epic Resins called their S7144 that's pretty bullet proof.
We use it on a relay board that goes into tractor trailer rigs air conditioning systems.
Steve
On Mon, May 3, 2021 at 3:56 PM Douglas Pauls < [log in to unmask]> wrote:
> Don't know Rich. Sounds like he is looking more for a potting material.
> ---
> *Douglas Pauls *| Technical Fellow | Electronics AMT
>
> *COLLINS AEROSPACE*
>
> 400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
>
> *Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
>
> [log in to unmask]
>
> [log in to unmask] for all Export Compliant Items
>
>
> On Mon, May 3, 2021 at 4:52 PM Richard Kraszewski <
> [log in to unmask]> wrote:
>
> > I will that a guess that the coating you are looking for is likely
> > parylene, or possibly a silicone coating.
> >
> > Rich Kraszewski
> > Plexus
> >
> > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * * This e-mail
> > and any attachments are confidential from Plexus Corp. and
> may
> > contain information which is privileged, confidential, and/or
> > protected
> by
> > non-disclosure agreements. They are intended solely for the use of
> > the named addressee(s). . Any unauthorized use or disclosure may
> > be unlawful. If you are not a named addressee, you must not use,
> > disclose, retain or reproduce all or any part of the information
> > contained in this e-mail or any attachments If you have received
> > this transmission in
> error,
> > please destroy it and notify us immediately by return e-mail or by
> calling
> > + 1 888 208 9005.
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Hatano
> > Sent: Monday, May 3, 2021 11:58 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] TechNet archives? looking for information on
> > coating or encapsulation long term protection
> >
> > <html><body><p style="background-color:#F5AD7C; border:1px solid
> > black;">[EXTERNAL] Use caution when clicking links or attachments
> > from unknown senders.</p><br></body></html> Excellent!!!
> > Thanks so much Steve.
> > I hope you have a great day!
> >
> > Richard Hatano
> > EDA Manager
> >
> > 3855 Ruffin Road, San Diego, CA 92123-1813 USA Direct 858-285-2392
> > | Fax 858-836-3400 [log in to unmask]
> >
> >
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> > Sent: Monday, May 3, 2021 9:56 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] TechNet archives? looking for information on
> > coating or encapsulation long term protection
> >
> > EXTERNAL SENDER – Exercise Caution.
> >
> >
> >
> > Hi Richard,
> >
> > It's still there, check out:
> >
> https://urldefense.com/v3/__https://ddei5-0-ctp.trendmicro.com:443/wis
> /clicktime/v1/query?url=https*3a*2f*2flinkprotect.cudasvc.com*2furl*3f
> a*3dhttp*253a*252f*252flistserv.ipc.org*252fscripts*252fwa.exe*253fIND
> EX*26c*3dE*2c1*2c*2d*5fjKsmkPzskGmh426O6bq8UU5N5sxYZ8e0MOY0D1SPtmrYUHQ
> wzmiQGij5*5fWcIr*5fNtyKbi4kVnCsYNz0wRb4i5NIsOGttWtHS4XSD5kovZnBv8SfgrW
> HI3l4*26typo*3d1&umid=E6764D8F-C16F-E005-9F9E-165AB66417E9&auth=fa0282
> dc3c44b189bcc708f19c936975d8469bfe-553ee348738739e35723801315099f645a0
> 3cc41__;JSUlJSUlJSUlJSUlJSUlJSUlJSUlJQ!!MvWE!VIfdjJP8qX-npQY-APqU1vxX8
> G2bS9Fro3BnE_Y8QPmrzarqhgGeWwxLlwkZ8YjqBQ$
> >
> > Steve
> >
> > On Mon, May 3, 2021 at 10:52 AM Richard Hatano <
> [log in to unmask]
> > >
> > wrote:
> >
> > > Hi,
> > >
> > > Sorry to trouble, but I just discovered that the IPC homepage no
> > > longer seems to have a link to the online forum archives (maybe I
> > > haven't checked in quite a while!).
> > > Are they now behind a registration wall?
> > > I was looking for information on best encapsulants (coatings
> > > aren't looking capable) to provide 100 year protection to passive
> > > circuitry that will be buried approx. 3-8 ft. underground inside a
> > > polypropylene
> > enclosure.
> > > I hope everyone is doing well and send thanks if anyone can help
> > > point me in the right direction.
> > >
> > > Richard Hatano
> > > EDA Manager
> > > [logo]
> > > 3855 Ruffin Road, San Diego, CA 92123-1813 USA Direct
> > > 858-285-2392
> > > | Fax 858-836-3400
> > > [log in to unmask]<mailto:[log in to unmask]>
> > >
> >
> >
> > --
> > Steve Gregory
> > Kimco Design and Manufacturing
> > Process Engineer
> > (208) 322-0500 Ext. -3133
> > Cell Phone: (918) 706-2779
> >
> > --
> >
> >
> >
> > This email and any attachments are only for use by the intended
> > recipient(s) and may contain legally privileged, confidential,
> > proprietary or otherwise private information. Any unauthorized use,
> > reproduction, dissemination, distribution or other disclosure of the
> > contents of this e-mail or its attachments is strictly prohibited.
> > If
> you
> > have received this email in error, please notify the sender
> > immediately and delete the original.
> >
> > <p></p>
> >
>
--
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133
Cell Phone: (918) 706-2779
--
This email and any attachments are only
for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
|