Subject: | |
From: | |
Reply To: | |
Date: | Fri, 22 May 2020 12:24:19 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
sorry, can't help. Doug is what you want. Feed him Mountain Dew he
will spill out gold....
jk
On May 21, 2020, at 8:49 PM, Wayne Thayer wrote:
> OK, I screwed up with the "Gentlemen" part. Firstly, there are many
> incredible females helping out on this forum, and Joyce Koo is
> among the
> finest of anyone who participates. Please accept my apologies.
>
> Joyce, any thoughts?
>
> Wayne Thayer
>
> On Wed, May 20, 2020 at 5:53 PM Wayne Thayer
> <[log in to unmask]> wrote:
>
>> Gentlemen-
>>
>> From J-STD-001, ROL1 must be cleaned, but then IPC/WHMA-A-620
>> declares
>> that solder sleeves are exempt from cleaning requirements. Why
>> don't the
>> extra halides cause problems if they are in a solder sleeve?
>>
>> TE Connectivity even has ROM1 available, which I guess is OK if it is
>> solid wire as opposed to stranded.
>>
>> Thanks,
>>
>> Wayne Thayer
>>
|
|
|