TECHNET Archives

January 2020

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 7 Jan 2020 10:02:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Further,

If the coupon/other surface to be examined is reflective there is no need to do an extraction process, you can get an excellent spectrum in reflection.

Regards,

Bev 

 

From: David Hillman <[log in to unmask]> 
Sent: Tuesday, January 7, 2020 9:54 AM
To: TechNet E-Mail Forum <[log in to unmask]>; [log in to unmask]
Subject: Re: [External] Re: [TN] [COM] Evaluating/Monitoring Silicone Contamination

 

Hi team! I second Bev's recommendation. We have used FTIR successfully for audit questions. You can take a clean metal coupon, place it in a cure oven, run a cure cycle and then conduct an FTIR assessment to demonstrate that no silicone cross contamination is occurring in the process (i.e. the coupon shows no indications of silicone material).

 

Dave Hillman

Collins Aerospace

[log in to unmask] <mailto:[log in to unmask]> 

 

On Tue, Jan 7, 2020 at 8:49 AM Bev Christian <[log in to unmask] <mailto:[log in to unmask]> > wrote:

Arnaud,
Not cheap, but FTIR is an excellent method for detecting silicones.
Regards,
Bev

-----Original Message-----
From: TechNet <[log in to unmask] <mailto:[log in to unmask]> > On Behalf Of GRIVON Arnaud
Sent: Tuesday, January 7, 2020 9:00 AM
To: [log in to unmask] <mailto:[log in to unmask]> 
Subject: [TN] [COM] Evaluating/Monitoring Silicone Contamination

Happy New Year TechNet !

Here is a first query for 2020...

We all know about the need of carefully segregate acrylic/urethane from
silicone conformal coatings, but how about evidencing and demonstrating (say
for an angry auditor) the actual lack of silicone cross-contamination on
toolings, ovens and workspaces ?

Are you aware of any reliable test system to perform silicone contamination
evaluations? What are their principles and related test methods & acceptance
criteria?

It looks like some suppliers offer Surface Silicone Contamination Test Kits
:

-          Henniker
Plasma<https://urldefense.proofpoint.com/v2/url?u=https-3A__plasmatreatment.co.uk_wp-2Dcontent_uploads_2016_09_Henniker-2DPla <https://urldefense.proofpoint.com/v2/url?u=https-3A__plasmatreatment.co.uk_wp-2Dcontent_uploads_2016_09_Henniker-2DPla&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Ep6e_JqIAB-C3jV3KJPdKGDQ5I2Fc3a2zsBHanP85-0&e=> &d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Ep6e_JqIAB-C3jV3KJPdKGDQ5I2Fc3a2zsBHanP85-0&e= 
sma-Technology-Overview.pdf> :
https://urldefense.proofpoint.com/v2/url?u=https-3A__plasmatreatment.co.uk_henniker-2Dplasma-2Dtechnology_products_surface-2Dte <https://urldefense.proofpoint.com/v2/url?u=https-3A__plasmatreatment.co.uk_henniker-2Dplasma-2Dtechnology_products_surface-2Dte&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=AB3yDQaPURrIweRZnP5pGgyVgrEDmkiS5qokssTFuP8&e=> &d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=AB3yDQaPURrIweRZnP5pGgyVgrEDmkiS5qokssTFuP8&e= 
st-equipment/test-for-surface-silicone-contamination/

-          Anderson Materials Evaluation :
https://urldefense.proofpoint.com/v2/url?u=http-3A__www.andersonmaterials.com_test-5Fmethods_testing-2Dfacilities-2Dfor-2Dsilicon <https://urldefense.proofpoint.com/v2/url?u=http-3A__www.andersonmaterials.com_test-5Fmethods_testing-2Dfacilities-2Dfor-2Dsilicon&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Zh_qyJmTEBherFBgLxWkxu6kfo-7GjsmgI8UlB50j9c&e=> &d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Zh_qyJmTEBherFBgLxWkxu6kfo-7GjsmgI8UlB50j9c&e= 
e-contamination.html#<https://urldefense.proofpoint.com/v2/url?u=http-3A__www.andersonmaterials.com_test-5Fmethods_testing-2D <https://urldefense.proofpoint.com/v2/url?u=http-3A__www.andersonmaterials.com_test-5Fmethods_testing-2D&d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Gt3ENH0EurLNosj337i8Yspnn4ckCubhDKFmlKaimZM&e=> &d=DwICAg&c=ilBQI1lupc9Y65XwNblLtw&r=qMshjwqeixvQjs1qYTl8aRebuaqi25nLzYlpmDF6tjI&m=0FRlP4dx1xpQpOzzzwM6Lve6zyjkRpbCgOTxviaD3Zk&s=Gt3ENH0EurLNosj337i8Yspnn4ckCubhDKFmlKaimZM&e= 
facilities-for-silicone-contamination.html>

Any practice of such test kits and return of experience to share?