> I should have been more precise in my answer. There is no way to add new
> "classes" of coating to the QPL. You can add new coatings in the current
> five material classes. A vendor would work with the QPL custodian to get
> their data package approved. The Defense Logistics Agency (DLA) is the
> custodian.
>
>
> https://landandmaritimeapps.dla.mil/programs/qmlqpl/QPLdetail.aspx?QPL=46058
>
>
>
> *Douglas Pauls *| Principal Materials and Process Engr | Advanced
> Operations Engineering
>
> *COLLINS AEROSPACE*
>
> 400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
>
> *Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
>
> [log in to unmask]
>
> [log in to unmask] for all Export Compliant Items
>
>
> On Fri, Sep 27, 2019 at 11:24 AM lduso - Diamond-MT.com <
> [log in to unmask]> wrote:
>
>> Must be some way. I see materials on it that were added in the last 5
>> years. If the spec is inactive, the QPL should be as well. Funny how
>> materials come and go on it.
>>
>> Lloyd Duso
>> General Manager
>> Diamond-MT
>> (814) 535-3505
>> www.Diamond-mt.com
>> <https://urldefense.proofpoint.com/v2/url?u=http-3A__www.Diamond-2Dmt.com&d=DwMFaQ&c=ilBQI1lupc9Y65XwNblLtw&r=lTRDjB8ojaf7ZaJ9DHeDAm7e-HFP9fxIkv6fRnV49HE&m=ULmmA2WSrPG-euMeY-deCLUWevVz89phHwj8frgjKfI&s=oFr-yoVP0WPp_VZiFAaHqHLexkvK7Dv25vmvncBVmWg&e=>
>>
>>
>> On Fri, Sep 27, 2019 at 11:01 AM Douglas Pauls <
>> [log in to unmask]> wrote:
>>
>>> Short answer - You Can't. The QPL goes with MIL-I-46058 and that has
>>> been
>>> inactive since 1995. They are "thinking" of revising it, but nothing to
>>> date.
>>> IPC-CC-830 has a procedure for adding new classes of coatings, which is
>>> found in IPC-CC-830 Rev C, Appendix D (I think).
>>>
>>> *Douglas Pauls *| Principal Materials and Process Engr | Advanced
>>> Operations Engineering
>>>
>>> *COLLINS AEROSPACE*
>>>
>>> 400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
>>>
>>> *Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
>>>
>>> [log in to unmask]
>>>
>>> [log in to unmask] for all Export Compliant Items
>>>
>>>
>>> On Fri, Sep 27, 2019 at 9:53 AM Richard Kraszewski <
>>> [log in to unmask]> wrote:
>>>
>>> > What is the process to get a new coating added to the QPL?
>>> > I haven't done this in a few (ok more than a few) years.
>>> > Is this still even possible?
>>> >
>>> > Rich Kraszewski
>>> > Senior Staff Process Engineer
>>> >
>>> > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>>> >
>>> > This e-mail and any attachments are confidential from Plexus Corp. and
>>> may
>>> > contain information which is privileged, confidential, and/or
>>> protected by
>>> > non-disclosure agreements. They are intended solely for the use of the
>>> > named addressee(s). . Any unauthorized use or disclosure may be
>>> > unlawful. If you are not a named addressee, you must not use,
>>> disclose,
>>> > retain or reproduce all or any part of the information contained in
>>> this
>>> > e-mail or any attachments If you have received this transmission in
>>> error,
>>> > please destroy it and notify us immediately by return e-mail or by
>>> calling
>>> > + 1 888 208 9005.
>>> >
>>>
>>
|