Hi,
As for grounding yea it depends, depends on where curents are flowing!
For non loose screws my understanding is Loctite, as in the RED.
Bob K.
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Campbell, Murray
Sent: Monday, September 30, 2019 5:52 PM
To: [log in to unmask]
Subject: Re: [TN] screws used for mounting circuit boards - so many choices
Hey Phil
Firm believer that all boards should be grounded directly to the chassis (if chassis mounted obviously) in which I put a copper pad around an unplated hole( to avoid any shredded copper burrs) The copper pad gets grounded to board chassis. We then mount the board with a flat washer, lock washer and screw.
If the board is grounded via wire harness, then ensure an unplated hole and mount with a flat washer, lock washer and screw. Copper pad not required.
MC
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nutting, Phil
Sent: Monday, September 30, 2019 3:25 PM
To: [log in to unmask]
Subject: [TN] screws used for mounting circuit boards - so many choices
Hi Technetters,
Over the years I have been involved in discussions about proper hardware to use when mounting circuit boards and if copper should be part of the stackup even if not a ground point.
I'll bet the answer is "it depends".
At one point we used a screw, split lock washer and a flat washer (labor intensive to assemble), then external tooth SEM screws that chewed up the FR-4. So we added a copper pad to act as a washer. SEM screws still chewed up the copper. With each of these we occasionally had units returned with loose screws. Enter nylon patch screws with no lock or flat washers but with a copper pad. No loose screws.
As time goes on there is someone that states the "standard" configuration uses a lock washer and flat washer and no copper.
I know there are SEM screws that incorporate a lock washer (star or split) with a flat washer, so that eliminates the assembly labor.
We make commercial OEM power supplies, no military stuff. So what do you use and why?
Phil Nutting | HVP Senior Development Engineer | Excelitas Technologies Corp
Lab: +1 978.224.4332 | Office: +1 978.224.4152
35 Congress St, Salem, MA 01970 USA
[log in to unmask]<mailto:[log in to unmask]>
www.excelitas.com<http://www.excelitas.com/>
[Excelitas R_emailsig]
Please consider the environment before printing this e-mail.
________________________________
This email message and any attachments are confidential and proprietary to Excelitas Technologies Corp. If you are not the intended recipient of this message, please inform the sender by replying to this email or sending a message to the sender and destroy the message and any attachments. Thank you.
“This message and/or attachments may include information subject to GD Corporate Policies 07-103 and 07-105 and is intended to be accessed only by authorized recipients. Use, storage and transmission are governed by General Dynamics and its policies. Contractual restrictions apply to third parties. Recipients should refer to the policies or contract to determine proper handling. Unauthorized review, use, disclosure or distribution is prohibited. If you are not an intended recipient, please contact the sender and destroy all copies of the original message.”
|