Short answer - You Can't. The QPL goes with MIL-I-46058 and that has been
inactive since 1995. They are "thinking" of revising it, but nothing to
date.
IPC-CC-830 has a procedure for adding new classes of coatings, which is
found in IPC-CC-830 Rev C, Appendix D (I think).
*Douglas Pauls *| Principal Materials and Process Engr | Advanced
Operations Engineering
*COLLINS AEROSPACE*
400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
*Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
[log in to unmask]
[log in to unmask] for all Export Compliant Items
On Fri, Sep 27, 2019 at 9:53 AM Richard Kraszewski <
[log in to unmask]> wrote:
> What is the process to get a new coating added to the QPL?
> I haven't done this in a few (ok more than a few) years.
> Is this still even possible?
>
> Rich Kraszewski
> Senior Staff Process Engineer
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp. and may
> contain information which is privileged, confidential, and/or protected by
> non-disclosure agreements. They are intended solely for the use of the
> named addressee(s). . Any unauthorized use or disclosure may be
> unlawful. If you are not a named addressee, you must not use, disclose,
> retain or reproduce all or any part of the information contained in this
> e-mail or any attachments If you have received this transmission in error,
> please destroy it and notify us immediately by return e-mail or by calling
> + 1 888 208 9005.
>
|
|
|