Hi Ben
I don't know about certified to IPC-4562 but if anyone is it would be
the Circuit Technology Center - they have been my go-to for this sort of
stuff. They can even do oddball custom stuff, I once had to repair some
radar parts that had a tapered trace, it had corroded off. Sent them a
drawing, got a replacement to match.
Graham Collins
Senior Process Engineer
Sunsel Systems
(902) 444-7867
On 9/5/2018 7:22 AM, Gumpert, Ben wrote:
> Technetters,
>
> Anyone have a good source of PWB repair materials (traces, pads, etc.) that are SnPb... AND don't have film adhesive... AND are certified to IPC-4562?
>
>
> Ben
|
|
|