Yup Real common for unsealed connectors.
You either have to find a better masking solution (often not possible) and/ or use multiple layers of a highly atomized (dry ) spray that is not very mobile when it hits the PCBA.
Some unsealed ZIF connector styles where the requirement is coat the leads but contacts are all KOZ are really a problem for me due to capillary action of the coating if still wet when it hits the PCBA.
Rich Kraszewski
Senior Staff Process Engineer
Plexus Engineering Solutions
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Wednesday, February 07, 2018 4:17 PM
To: [log in to unmask]
Subject: Re: [TN] IPC-CC-830 (Conformal Coat)
sorry for the long delay (and thank you for the responses) but as I was reviewing these posts I had another question:
Have you ever heard of problems with conformal coating material wicking up the connector leads and causing intermittent connections?
thanks again,
Jack
On Wed, 6 Dec 2017 14:09:46 -0500, lduso - Diamond-MT.com <[log in to unmask]> wrote:
(..snip...)
>It's up to me to decide how close to J1 to get with the coating. I once
>coated the leads of all the fine-pitch connectors and the customer said
>that was too close. The next customer will reject the work if I don't
>coat the leads.
|
|
|