TECHNET Archives

February 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Thu, 8 Feb 2018 03:01:15 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Message-ID:
Subject:
From:
Richard Kraszewski <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Yup  Real common for  unsealed connectors. 



You either have to find a better masking solution (often not possible) and/ or use  multiple layers of a highly atomized  (dry ) spray that is not very mobile  when it hits  the PCBA. 



Some unsealed  ZIF connector styles where the requirement is coat the leads but contacts are all KOZ are really a problem  for me due to capillary action of the coating if still wet when it hits the PCBA. 







Rich  Kraszewski 

Senior Staff Process Engineer

Plexus Engineering Solutions 

* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *



This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements.  They are intended solely for the use of the named addressee(s).  .  Any unauthorized use or disclosure may be unlawful.  If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson

Sent: Wednesday, February 07, 2018 4:17 PM

To: [log in to unmask]

Subject: Re: [TN] IPC-CC-830 (Conformal Coat)



sorry for the long delay (and thank you for the responses) but as I was reviewing these posts I had another question:



Have you ever heard of problems with conformal coating material wicking up the connector leads and causing intermittent connections?



thanks again,

Jack





On Wed, 6 Dec 2017 14:09:46 -0500, lduso - Diamond-MT.com <[log in to unmask]> wrote:



(..snip...)

>It's up to me to decide how close to J1 to get with the coating. I once 

>coated the leads of all the fine-pitch connectors and the customer said 

>that was too close. The next customer will reject the work if I don't 

>coat the leads.