un controlled thermal shock (uncontrolled RH)... elevator type...
with upper temp less than 85 C (residence time for the molecule at
high temp is too short to form any ingress... and another one is
pressure cooker test...
On Nov 22, 2017, at 5:46 PM, Richard Kraszewski wrote:
> Other than what is written in IPC CC830 for thermal shock and MIR
> testing , is anyone away of any industry standard that addresses
> the functionality of coating or devices when exposed to
> condensation?
>
> I have looked at the IP Code for water ingress but all of that
> water testing seems too invasive & harsh for what I am looking for.
>
> https://en.wikipedia.org/wiki/IP_Code
>
> Something in IEC perhaps.
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Plexus Engineering Solutions
>
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
>
> This e-mail and any attachments are confidential from Plexus Corp.
> and may contain information which is privileged, confidential, and/
> or protected by non-disclosure agreements. They are intended
> solely for the use of the named addressee(s). . Any unauthorized
> use or disclosure may be unlawful. If you are not a named
> addressee, you must not use, disclose, retain or reproduce all or
> any part of the information contained in this e-mail or any
> attachments If you have received this transmission in error, please
> destroy it and notify us immediately by return e-mail or by calling
> + 1 888 208 9005.
|
|
|