un controlled thermal shock (uncontrolled RH)... elevator type... with upper temp less than 85 C (residence time for the molecule at high temp is too short to form any ingress... and another one is pressure cooker test... On Nov 22, 2017, at 5:46 PM, Richard Kraszewski wrote: > Other than what is written in IPC CC830 for thermal shock and MIR > testing , is anyone away of any industry standard that addresses > the functionality of coating or devices when exposed to > condensation? > > I have looked at the IP Code for water ingress but all of that > water testing seems too invasive & harsh for what I am looking for. > > https://en.wikipedia.org/wiki/IP_Code > > Something in IEC perhaps. > > Rich Kraszewski > Senior Staff Process Engineer > Plexus Engineering Solutions > > > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * * > > This e-mail and any attachments are confidential from Plexus Corp. > and may contain information which is privileged, confidential, and/ > or protected by non-disclosure agreements. They are intended > solely for the use of the named addressee(s). . Any unauthorized > use or disclosure may be unlawful. If you are not a named > addressee, you must not use, disclose, retain or reproduce all or > any part of the information contained in this e-mail or any > attachments If you have received this transmission in error, please > destroy it and notify us immediately by return e-mail or by calling > + 1 888 208 9005.