TECHNET Archives

November 2017

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Giamis, Andy" <[log in to unmask]>
Date:
Fri, 17 Nov 2017 06:10:25 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Message-ID:
Subject:
From:
David Hillman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (28 lines)
Hi Andy - I have some stuff in my files which I'll send you once I get to
the office (first part of today is a Rockwell Roadshow where we feed LN2
frozen marsh mellows to students and other fun science stuff!). Do a search
for Wally Bader's classic dissolution work - its for tin/lead and not tin
but it would give you a pretty good first order estimate. Also look in the
American Welding Society (AWS) Soldering Handbook - I believe Paul Vianco
has data in that reference. Is there a specific noble metal of interest?

Dave Hillman
Rockwell Collins
[log in to unmask]

On Thu, Nov 16, 2017 at 10:48 PM, Giamis, Andy <[log in to unmask]>
wrote:

> I’m looking for a reference showing the dissolution rates and temperature
> dependence of noble metals in tin.
>
> A wise man (wise guy, AKA George) used to always carry two things: an IKEA
> measuring tape and a great chart showing this data.
>
> I’ve searched Wikigooglepedia and have been through my 2006 CRC handbook
> (Phys and Chem) and several solid state texts.
>
> Thanks
> Andy
>