TECHNET Archives

December 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Wed, 14 Dec 2016 10:45:05 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Message-ID:
Subject:
From:
David Hillman <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (79 lines)
Hi Ioan - sorry, I don't have any information on the wire pull portion of
your task.

Dave

On Wed, Dec 14, 2016 at 10:43 AM, Ioan Tempea <
[log in to unmask]> wrote:

> Thanks Dave,
>
> I knew you guys were doing a good job in those committees!
>
> Anything on wire pull, except Dage?
>
> Best regards,
>
> Ioan
>
> De : David Hillman [mailto:[log in to unmask]]
> Envoyé : Wednesday, December 14, 2016 10:59 AM
> À : TechNet E-Mail Forum; Ioan Tempea
> Objet : Re: [TN] Mechanical test equipment for MIL-883 methods 2003 and
> 2004
>
> Hello Ioan - look in the back of the IPC JSTD 002 specification, Appendix
> E. There is solderability equipment information listed there in that
> Informative Annex.
>
> Dave Hillman
> Rockwell Collins
> IPC-JSTD-002 chairman
>
> On Wed, Dec 14, 2016 at 8:14 AM, Ioan Tempea <[log in to unmask]
> com<mailto:[log in to unmask]>> wrote:
> Dear Technos,
>
> I need to test solderability (per J-STD-002 and method 2003, test B, of
> the 883) and lead integrity (method 2004 condition D of the 883) for
> leadless components.
>
> Can you, please, suggest equipment for :
>
> *         Steam aging
>
> *         Solder bath dipping
>
> *         Wire pull; this one is for method 2004, I wonder if anybody is
> using regular wire pulling machine (normally used for wire bonds) for this
> task.
>
> Thank you,
>
> Ioan Tempea, P. Eng.
> Manufacturing Engineer, Satellite Systems
>
> [cid:[log in to unmask]]
>
> MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada
> Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
> Tel: +1-514-457-2150 x3556<tel:%2B1-514-457-2150%20x3556>
> www.mdacorporation.com<http://www.mdacorporation.com><http:/
> /www.mdacorporation.com/>
>
> This e-mail, and any attachments, are intended solely for the use of the
> intended recipient(s) and may contain legally privileged, proprietary
> and/or confidential information. Any use, disclosure, dissemination,
> distribution or copying of this e-mail and any attachments for any purposes
> that have not been specifically authorized by the sender is strictly
> prohibited. If you are not the intended recipient, please immediately
> notify the sender by reply e-mail and permanently delete all copies and
> attachments. This email is for informational purposes only and shall not be
> interpreted to authorize or conclude a binding agreement between MDA and
> any other party unless this email contains or is accompanied by an express
> written confirmation of MDA's intention to enter into a binding agreement,
> such confirmation shall only be provided by an authorized representative of
> MDA.
>
>

ATOM RSS1 RSS2