not reliably. but you can do it withstand initial pull strength if you
smash it. based on my understanding...
jk
> Hi All,
> Is it possible to wire bond when the finish is gold over copper - no
> nickel? Thanks. Steve Kelly
>
> Phone(O) (416) 750-8433
> Phone (C) (416) 577-8433
>
> If the recipient to whom this e-mail is sent has an NDA with PFC Flexible
> Circuits Limited this e-mail is considered confidential and is subject to
> any NDA agreements between the respective parties.
>
> See PFC on "How its' Made" in Canada on July 7th at 8 p.m. on the
> Discovery Channel
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________