Hi team - thanks to everyone for the recommendations and suggestions. We
had already begun some trials with the temporary mask material but I wanted
to double check if any other possibilities existed. Wayne - the reason for
the "temporary" caveat was that if I use a permanent material such as an
edgebond adhesive, I potential may be required to conduct testing as the
assembly configuration would be different than what was ran thru
qualification testing. If I can find a temporary mask option, I can avoid
having to deal with those aspects of the topic.
TechNet is such an awesome resource!
Dave
On Tue, Dec 9, 2014 at 8:09 AM, Wayne Thayer <[log in to unmask]> wrote:
> Seems like perfect use for a staking adhesive, except for your strange
> requirement that it be easily removable. Staking adhesives enhance
> reliability
> by assisting with strengthening the mechanics at the corner balls, and are
> known to increase the resistance to shock loads too.
>
> So if you're stuck with this strange set of requirements, then I doubt
> you'll
> find something pre-qualified for it. So since qualification is required,
> anything is open game. I'd play with water washable solder masking
> materials,
> also peelable masking material.
>
> Wayne Thayer
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
> Sent: Tuesday, December 09, 2014 8:42 AM
> To: [log in to unmask]
> Subject: [TN] BGA Reflow Issue
>
> Hi gang - looking for an adhesive suggestion. I have an assembly in which a
> heavy BGA was accidently located on process side one (bottom) so that when
> we
> reflow process side two (top) the BGA is doing its best to fall off.
> Unfortunately I can't reverse my process order for a couple of reasons so
> I am
> looking for a temporary fix until I can get the assembly revised. I was
> thinking of using some type of adhesive to temporarily hold the BGA in
> place
> during reflow - tack down the corners sort of action. Does anyone have any
> adhesive (ideally temporary, water washable/removable) suggestions I can
> investigate?
>
> TIA
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|