Good day TechNet
We are a late arrival to the lead-free party, as our customers thus far
are exempt. But a couple of them see the writing on the wall and are
moving toward RoHS compliance. Which leads me to two questions with
regards to our testing of parts to ensure compliance.
The first question - what XRF? We are concerned with price given that
we are dipping our feet here, does anyone have a recommendation for a
good but inexpensive unit?
Second question is concerning alternative test methods, a customer is
planning to use 3M LeadCheck swabs (LC-8S10C) to ensure no lead. Given
that the product is described as for use on painted surfaces I don't
think this is intended as a way to verify lead-free status on
electronics. Any comments on this?
Thanks!
--
regards,
Graham Collins
Senior Process Engineer
Sunsel Systems
(902) 444-7867 ext 211
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|