TECHNET Archives

July 2014

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 25 Jul 2014 18:27:04 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Message-ID:
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
Hi Victor-

 

No, I don't know of direct IPC standards on this. I'd think it would be in
the specification for your laminate (such as FR4). The laminates probably
list a maximum resin weight percentage. But that would be for the whole
shebang, obviously that falls apart when you get into a small enough area.

 

Just how small are you talking about?

 

Reasons for it happening:

-High flow pre-preg with very uneven metal loading from a vertical
perspective. (Unbalanced layer-to-layer unevenness results in warpage, but
if you had a whole lot of metal with edges all ending in the same spot on
each layer, then the resin would be displaced to the areas with less
copper.)

-Cutouts in pre-preg to accommodate cavities or other special structures.

-Poorly made laminate/prepreg. In that case, it should fail the spec on
resin weight percentage.

 

Wayne

 

From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Friday, July 25, 2014 1:26 PM
To: [log in to unmask]; Wayne Thayer
Cc: [log in to unmask]
Subject: RE: PWB, rich epoxy area witin laminate

 

Wayne,

 

   Are you aware of any IPC STDs which cover this anomaly or even bench
marking?  I hope PWB/PCB gurus will chime in on this topic.

 

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Thursday, July 24, 2014 3:44 PM
To: [log in to unmask]
Subject: Re: [TN] PWB, rich epoxy area

Resin rich will be weaker, lower dielectric constant, more subject to
cracking, higher coefficient of expansion. Actual effect on
reliability/product use depends on how close the design relies on "normal"
laminate specs.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, July 24, 2014 3:37 PM
To: [log in to unmask]
Subject: [TN] PWB, rich epoxy area

Fellow TechNetters:

Can a rich epoxy area/site within a PWB laminate be harmful. What can
happen and what could be the reason for the rich epoxy area? Where can I
fins supporting literature in IPC STDs and or bench marking.

Victor,

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]