Sender: |
|
X-To: |
|
Date: |
Fri, 25 Jul 2014 12:25:33 -0500 |
Reply-To: |
|
Subject: |
|
MIME-Version: |
1.0 |
Message-ID: |
|
Content-Transfer-Encoding: |
quoted-printable |
Content-Type: |
text/plain; charset="us-ascii" |
From: |
|
Parts/Attachments: |
|
|
Wayne,
Are you aware of any IPC STDs which cover this anomaly or even bench marking? I hope PWB/PCB gurus will chime in on this topic.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Thursday, July 24, 2014 3:44 PM
To: [log in to unmask]
Subject: Re: [TN] PWB, rich epoxy area
Resin rich will be weaker, lower dielectric constant, more subject to cracking, higher coefficient of expansion. Actual effect on reliability/product use depends on how close the design relies on "normal"
laminate specs.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Thursday, July 24, 2014 3:37 PM
To: [log in to unmask]
Subject: [TN] PWB, rich epoxy area
Fellow TechNetters:
Can a rich epoxy area/site within a PWB laminate be harmful. What can
happen and what could be the reason for the rich epoxy area? Where can I
fins supporting literature in IPC STDs and or bench marking.
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|