Back in the 80's I was working with what was considered "high density" boards (Burroughs Corporation memory boards) with Sn/Pb traces. Where the soldermask wrinkled on parallel traces, occasionally a small fissure occurred below the surface allowing a fine whisker of solder to cause a short. This wasn't CAF as it was detected immediately (<5 min.) after wave/clean. SMOBC (very difficult to find a supplier capable of this process at the time) solved the problem.
Moral of the story: Be sure the electrical clearances are adequate.
Ed Popielarski
Engineering Manager
970 NE 21st Ct.
Oak Harbor, Wa. 98277
Ph: 360-675-1322
Fx: 206-624-0695
Cl: 949-581-6601
“It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design.”
https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&spn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ahne Oosterhof
Sent: Monday, May 05, 2014 9:58 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask over Tin Lead Plating
That is 'correct'.
Ahne.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: 5 May, 2014 05:15
To: [log in to unmask]
Subject: Re: [TN] Solder Mask over Tin Lead Plating
This was common practice in the days before SMT. The masks used at the time would ripple where the tracks were reflowed, but didn't crack. Still made it through the solder wave just fine, and no problem with hand soldering either.
I sometimes still see this today with single sided wave soldered boards such as cheap consumer audio and power supplies.
"Correct" is what works for your application. Inherently, there is no reliability issue with this construct.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ramakrishnan Saravanan
Sent: Sunday, May 04, 2014 4:18 AM
To: [log in to unmask]
Subject: [TN] Solder Mask over Tin Lead Plating
Hi,
We received few PCBs from an European PCB manufacturer for Aerospace Industry.
I am surprised to see Solder Mask is applied over tin lead plated tracks. My understanding is if u do reflow , the solder under the mask will melt and affect the mask. The correct method is applying Soldermask over bare copper isn't?. Kindly advise. regards,
R.Saravanan
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|