I only have seen some "suspected" occurrence of this.
Somewhat dependant on how much is deposited, was the tape baked, and if you have an aromatic solvent based coating. The latter can extract some adhesive from the tape perimeter.
You can however use Si based tape and never have issues.
I personally think that is tendency to over react to the term silicone. That is due to hand-soldering where we all learn that silicone hand lotions hamper solderability (which they can), and older Si Ccings that use some rather obsolete cure catalyst mechanisms.
Rich Kraszewski
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, August 06, 2013 8:18 AM
To: [log in to unmask]
Subject: [TN] Silicone adhesives on tapes
Do you think the silicone adhesive on Kapton and Shercon tapes can create a manufacturing issue during conformal coating or for sensitive electronics?
Doug, I would be especially interested in your respected input on this question.
This message and/or attachments may include information subject to GDC4S S.P. 1.8.6 and GD Corporate Policy 07-105 and are intended to be accessed only by authorized recipients. Use, storage and transmission are governed by General Dynamics and its policies. Contractual restrictions apply to third parties. Recipients should refer to the policies or contract to determine proper handling. Unauthorized review, use, disclosure or distribution is prohibited. If you are not an intended recipient, please contact the sender and destroy all copies of the original message.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|