I have thick skin.....
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Wednesday, July 17, 2013 10:37 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating
Victor,
I was picking on George there, not you.
Best Regards,
Andy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Wednesday, July 17, 2013 10:29 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating
Reminds me of a scene from Taxi
Rev. Jim (studying for a driving test): "What does a yellow light mean?"
Alex: "Slow down."
Rev. Jim: "What does a yellow light mean"
Alex: "Slow down."
Rev. Jim: "Okie Dokie. W h a t d o e s a y e l l o w l i g h t m e a n"
Best Regards,
Andy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M. [Contractor]
Sent: Wednesday, July 17, 2013 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating
No
Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail: [log in to unmask]
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, July 17, 2013 9:50 AM
To: [log in to unmask]
Subject: [TN] Bright tin Plating, electrolytic plating
Fellow TechNetters:
Is electrolytic bright tin plating self-limiting in thickness?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|