TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 17 Jul 2013 10:54:17 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Victor Hernandez <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (87 lines)
I have thick skin.....

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Wednesday, July 17, 2013 10:37 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating

Victor,
I was picking on George there, not you.  

Best Regards,
Andy


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Giamis, Andy
Sent: Wednesday, July 17, 2013 10:29 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating

Reminds me of a scene from Taxi

Rev. Jim (studying for a driving test): "What does a yellow light mean?"

Alex: "Slow down."

Rev. Jim: "What   does   a   yellow   light    mean"

Alex: "Slow down."

Rev. Jim: "Okie Dokie.  W h a t   d o e s    a   y e l l o w   l i g h t    m e a n"

Best Regards,
Andy


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M. [Contractor]
Sent: Wednesday, July 17, 2013 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Bright tin Plating, electrolytic plating

No

Regards,
George
George M. Wenger
Failure Signature & Characterization Lab LLC
609 Cokesbury Road, High Bridge, NJ 08829
(908) 638-8771 Home (732) 309-8964 Mobile
E-mail: [log in to unmask]
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Wednesday, July 17, 2013 9:50 AM
To: [log in to unmask]
Subject: [TN] Bright tin Plating, electrolytic plating

Fellow TechNetters:

   Is electrolytic bright tin plating self-limiting in thickness?

Victor,

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2