TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 11 Jun 2013 19:24:44 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Phil Bavaro <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (17 lines)
Doug et al,

Is there a disagreement in the industry as to what minimum thickness of urethane is required in order to mitigate tin whisker concerns?

I am hearing that the .003+/-.002" does not provide enough of a minimum thickness and that the number is as high as .004".   I can understand wanting the minimum being raised to .002" but higher than that would seem to make the process much more difficult to control.

I have a potential customer asking if we measure the thickness on the individual component leads which is another can of worms it seems.  We always used flat samples to document our thicknesses.

I did not get to attend this years APEX so I might have missed the latest data.
________________________________
 This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2