Phil,
While this is an answer I "should" know, I don't. Dave Hillman regularly
attends and presents at the CALCE yearly conference on whiskers and so he
keeps up on all of that. At present, my esteemed colleague is bumping his
head on rocks, kayaking upside down, on some white water in North
Carolina. He should be back in the office on Monday and will no doubt
answer then.
From our discussions, the general rule is still "no conformal coating
prevents whiskers". A thicker coating may cause the whisker to expend
more energy punching through and yet more energy to punch through an
adjacent coating on a lead (usually resulting in buckling), but I have yet
to hear about some magic thickness of any kind of coating that completely
mitigates whiskers. But I could be wrong.
Dave?
Doug Pauls
From: Phil Bavaro <[log in to unmask]>
To: <[log in to unmask]>
Date: 06/11/2013 02:26 PM
Subject: [TN] minimum thickness of Type UR Conformal coat and tin
whiskers
Sent by: TechNet <[log in to unmask]>
Doug et al,
Is there a disagreement in the industry as to what minimum thickness of
urethane is required in order to mitigate tin whisker concerns?
I am hearing that the .003+/-.002" does not provide enough of a minimum
thickness and that the number is as high as .004". I can understand
wanting the minimum being raised to .002" but higher than that would seem
to make the process much more difficult to control.
I have a potential customer asking if we measure the thickness on the
individual component leads which is another can of worms it seems. We
always used flat samples to document our thicknesses.
I did not get to attend this years APEX so I might have missed the latest
data.
________________________________
This message and any attachments are solely for the use of the addressee
and may contain L-3 proprietary information that may also be defined as
USG export controlled technical data. If you are not the intended
recipient, any disclosure, use or distribution of its content is
prohibited. Please notify the sender by reply e-mail and immediately
delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|