TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 7 May 2013 16:18:17 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Goodyear, Patrick" <[log in to unmask]>
Message-ID:
Subject:
From:
"Goodyear, Patrick" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (61 lines)
Foreign material contamination maybe, oily residue from manufacturing process?  Is it the same place on all boards that fail to wet?   

pat

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 07, 2013 8:48 AM
To: [log in to unmask]
Subject: [TN] Irritating ENIG Non-wetting

Hi All,

 

We just were running some boards (ENIG finished) where we're seeing this sporadic non-wetting on some of the pads:

 

http://stevezeva.homestead.com/PKG2.jpg

 

http://stevezeva.homestead.com/PKG3.jpg

 

http://stevezeva.homestead.com/PKG4.jpg

 

Usually it's just a few pads and the rest of the board is fine. We get the boards in packs of 20, and it's only a couple or so out of the pack that exhibit the problem. It's just enough to be irritating.

 

When we touch the locations up with a soldering iron they wet fine.
We're using a 63/37 water soluble paste, and the problem doesn't confine itself to just certain pads or parts, it's random.

 

Like I said it's just enough to be irritating.....   /:o[

 

Steve Gregory

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


PG&E is committed to protecting our customers' privacy. 
To learn more, please visit http://www.pge.com/about/company/privacy/customer/

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2