Foreign material contamination maybe, oily residue from manufacturing process? Is it the same place on all boards that fail to wet?
pat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, May 07, 2013 8:48 AM
To: [log in to unmask]
Subject: [TN] Irritating ENIG Non-wetting
Hi All,
We just were running some boards (ENIG finished) where we're seeing this sporadic non-wetting on some of the pads:
http://stevezeva.homestead.com/PKG2.jpg
http://stevezeva.homestead.com/PKG3.jpg
http://stevezeva.homestead.com/PKG4.jpg
Usually it's just a few pads and the rest of the board is fine. We get the boards in packs of 20, and it's only a couple or so out of the pack that exhibit the problem. It's just enough to be irritating.
When we touch the locations up with a soldering iron they wet fine.
We're using a 63/37 water soluble paste, and the problem doesn't confine itself to just certain pads or parts, it's random.
Like I said it's just enough to be irritating..... /:o[
Steve Gregory
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
PG&E is committed to protecting our customers' privacy.
To learn more, please visit http://www.pge.com/about/company/privacy/customer/
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|