TECHNET Archives

April 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Gregg Owens <[log in to unmask]>
Date:
Thu, 4 Apr 2013 15:39:30 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (36 lines)
Hmmm, not sure what would be the impact if you use it in vacuum.  Better not ;-).  

Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Owens
Sent: Thursday, April 04, 2013 10:38 AM
To: [log in to unmask]
Subject: [TN] Butane Soldering Irons

Since we hand solder outside of the normal manufacturing floor, our technicians are requesting to use a butane soldering iron. I have no previous experience with this type of soldering iron. With a temperature setting of 1076°F it seems rather high and potentially damaging to resulting solder connection, insulation, people, etc.

http://www.apexhandtools.com/brands/CF_Files/model_detail.cfm?upc=037103060976

Any thoughts from experience would be most appreciated.

Gregg

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2