Also, Ioan, check IPC 7711-7721. It has some really good info on conformal coat removal methods, including a chart by coating type and the corresponding method of removal that is recommended.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
Sent: Wednesday, October 10, 2012 12:48 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal coating removal
GDAIS Security Warning:
This message was delivered from the Internet. Be cautious about trusting the content, particularly any links or attachments.
If there is any doubt as to the authenticity, forward this email as an attachment to [log in to unmask] for analysis prior to opening any attachment or link.
I totally agree with Dewey on this. I am not sure where Dewey was going with partial coating and stripping but..
..strip and re-coat will be faster and more effective. Having run our own coating service for many years, mucking around with "thousands of boards" is going to cause more trouble than it solves.
For example, you locally remove the coating (or solder through) then you have re-solder the replacement component so how are you going to effectively clean the surrounding area - especially given that the low surface energy of the cleaning solvent will take it everywhere?
Chemically strip - de-solder - replace component and re-solder - clean - re-coat. Job done..
.they even have a new coat to show off when they get back into service. Be careful that your partial new coat doesn't become a fur!
Graham - Beau Brummel - Naisbitt
On 11 Oct 2012, at 01:16, Whittaker, Dewey (EHCOE) wrote:
> I would wait for Doug on this, since he takes his lead from Graham on sartorial splendor and is more used to partially coated affairs. I would strip the whole assembly if possible as the process does an excellent job of prepping the substrate for re-coating.
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
> Sent: Wednesday, October 10, 2012 9:56 AM
> To: [log in to unmask]
> Subject: [TN] Conformal coating removal
>
> Dear Technos,
>
> We need to locally strip the acrylic coating (1B31S) from a few components, on a few thousands of boards. Right now we're using Q-tips to do the rubbing and, besides having to pluck tons of fibers afterwards, we're also going through a lot of Q-tips.
>
> So the question is: is there anything else we can use, that will be more effective, cleaner and more economical?
>
> Thank you,
>
> Ioan Tempea
> Ingénieur principal de fabrication / Senior Manufacturing Engineer
> [signature002]<http://www.digico.cc/>
>
> 950 RUE BERGAR, LAVAL, QC, H7L 5A1<http://g.co/maps/2gh3f>
> T+ 1 (450) 967-7100, EXT244
> ----------------------------------------------------------------------
> -- [signature001] <http://www.facebook.com/pages/Digico/277076778479>
> ----------------------------------------------------------------------
> -- Lauréat Dunamis 2012<http://digico.cc/dunamis-2012/>
> Entreprise manufacturière / Gestion du capital humain
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|