Should be able to solder directly to iron in S/S as long as there is no thick passivation layer or surface chemical enhancement....
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, September 28, 2012 10:33 AM
To: [log in to unmask]
Subject: Re: [TN] soldering stainless steel
Perhaps a nickel under plate?
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGrath, Jim
Sent: Friday, September 28, 2012 12:00 PM
To: [log in to unmask]
Subject: Re: [TN] soldering stainless steel
Preplate the solder area with Sn or SnPb. You may need a copper underplate.
Jim McGrath
Strategic Marketing Manager
TE Consumer Devices
Cell: 630-244-3872
Email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge
Sent: Friday, September 28, 2012 10:17 AM
To: [log in to unmask]
Subject: [TN] soldering stainless steel
Hi all,
has anybody experience with soldering stainless steel parts directly on a PCB? What solder process work fine?
Application is a medical sensor with body contacts.
Torsten
Kind regards
KRISTRONICS GmbH
Torsten Hagge
Gewerbegrund 5-9
24955 Harrislee
Telefon +49 (0) 461 7741-624
Telefax +49 (0) 461 7741-642
[log in to unmask]
www.kristronics.de
Meet at electronica 2012, A6, 409
Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL Geschäftsführer Dipl.-Ing. oec. Thormod Ohm Ust-Id-Nr. DE 811182059
Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|