Torsten,
The last time I did this type of thing I did the following:
Pre-tin S/S soldering areas with the same solder metallurgy as your solder paste using a very active acid flux (I used a hydrobromic acid type flux), wash thoroughly, then place on PCB like regular component and/or RF shield...
Some adjustment need to be made depending (that word again...) on the joint configuration and part...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge
Sent: Friday, September 28, 2012 8:17 AM
To: [log in to unmask]
Subject: [TN] soldering stainless steel
Hi all,
has anybody experience with soldering stainless steel parts directly on a PCB? What solder process work fine?
Application is a medical sensor with body contacts.
Torsten
Kind regards
KRISTRONICS GmbH
Torsten Hagge
Gewerbegrund 5-9
24955 Harrislee
Telefon +49 (0) 461 7741-624
Telefax +49 (0) 461 7741-642
[log in to unmask]
www.kristronics.de
Meet at electronica 2012, A6, 409
Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL
Geschäftsführer Dipl.-Ing. oec. Thormod Ohm
Ust-Id-Nr. DE 811182059
Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011
IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|