TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge Hernefjord <[log in to unmask]>
Date:
Thu, 16 Feb 2012 20:02:13 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (57 lines)
Key point is gas tight.  Ag/AgO/AgO2 all conductive, perfect for contact with absence of S, Cl, etc.  Ag-Pd also being used in the past.  If you use higher current, connector is easy to get good performance (not the extremely high current).  If it is low voltage, low current, stay with gold.  

Joyce Koo
Materials Researcher - Materials Interconnect Lab
Research In Motion Limited
Office: (519) 888-7465 79945
Mobile: (226) 220-4760

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Thursday, February 16, 2012 1:37 PM
To: [log in to unmask]
Subject: Re: [TN] Silver immersion with gold fingers

Not an answer on your question.
( Actually, I wonder if not one could use silver all over. Many years back
a lot of manufacturers had silver fingers. Together with correctly designed
connector forks, the contact points were gas tight, and there was no
 problem with connection reliability. If the boards will be slided in/out
several times, you need of course thicker silver than the std ImAg.
Wouldn't that be worth a study now when gold is extremly expensive.?)

My two sixpence

Inge



On 10 February 2012 16:48, John Burke <[log in to unmask]>wrote:

> Having some issues with silver immersion on a board with gold pated
> fingers - anyone having success with this?
>
> Issue apparently is in masking off the gold during the silver process.
>
> John
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2