Key point is gas tight. Ag/AgO/AgO2 all conductive, perfect for contact with absence of S, Cl, etc. Ag-Pd also being used in the past. If you use higher current, connector is easy to get good performance (not the extremely high current). If it is low voltage, low current, stay with gold. Joyce Koo Materials Researcher - Materials Interconnect Lab Research In Motion Limited Office: (519) 888-7465 79945 Mobile: (226) 220-4760 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord Sent: Thursday, February 16, 2012 1:37 PM To: [log in to unmask] Subject: Re: [TN] Silver immersion with gold fingers Not an answer on your question. ( Actually, I wonder if not one could use silver all over. Many years back a lot of manufacturers had silver fingers. Together with correctly designed connector forks, the contact points were gas tight, and there was no problem with connection reliability. If the boards will be slided in/out several times, you need of course thicker silver than the std ImAg. Wouldn't that be worth a study now when gold is extremly expensive.?) My two sixpence Inge On 10 February 2012 16:48, John Burke <[log in to unmask]>wrote: > Having some issues with silver immersion on a board with gold pated > fingers - anyone having success with this? > > Issue apparently is in masking off the gold during the silver process. > > John > > ______________________________________________________________________ > This email has been scanned by the Symantec Email Security.cloud service. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________