TECHNET Archives

January 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 10 Jan 2012 09:56:21 +0000
Reply-To:
Message-ID:
<3DE6C49EBEE94735B8136A2AC9FDB02C@MikeLaptop>
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (127 lines)
These gibberish mails look like a text rendering of a formatted document. So possibly it's to do with how sender's Email is set up. If so the answer is to send only plain text mail to TechNet. [I seem to recall that some time ago this was the default for the entire forum.]
In MS Outlook you can certainly select to send plain text rather than RTF or HTML when originating a mail. The specifics of how to do this will depend on your version. In some versions you can adjust the contact's properties in your address/contacts folder. Or you can change format in an individual mail. Or just start a new mail to TechNet and then right click on the address in the to line, select Outlook properties and then change Internet properties to "use Plain text" instead of "let Outlook decide." This will take effect the next time you reply - like this. :) 



Regards

Mike Fenner 
Bonding Services & Products
T: +44 [0] 1865 522 663 E: [log in to unmask]

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: Tuesday, January 10, 2012 9:04 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux?

Rex,

Wow, you certainly received much less gibberish than I!  Am I the only one to receive total gibberish?  Meaning, something on my end?

Joyce once indicated that she was at an outside [of the plant] WiFi hotspot when one of hers came in garbled.

Steve C

-----Original Message-----
From: Rex Waygood [mailto:[log in to unmask]] 
Sent: Tuesday, January 10, 2012 3:58 AM
To: TechNet E-Mail Forum; Steven Creswick
Subject: RE: [TN] Cleaning water soluble flux?

I could read most of it but part of the first line was odd.
This seems to be a problem that is occurring more often.
What do we need to do to avoid the problem? 
Rex


‰?z{S­©?}ê?? ?x j??à*'µé?O*^µ?m?™Z?w!j» • §vŒ,×nzHi Joyce -  you can accurately measure the amount of moisture in a pwb using a Mettler or equivalent 4 digit accuracy balance. The procedure to do so must be very very controlled and rigidly followed. The IPC-1601 standard lists the protocol for the procedure. We use have used this protocol successfully for many years producing data we use in our production facilities on a daily basis. I would love to have 6 digit sensitivity for the task but that isn't always available or completely necessary.

On a separate note -  the cleaning debate shouldn't be about if there is water left on a pwa after blowing it off. As Terry and others have detailed, the real issue is what contaminates are left in the laminate or the soldermask after the tap water or cleaning solution has been removed. 
There is an immense amount of published data on the subject so there is no need to run another test.

Dave Hillman
Rockwell Collins
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Creswick
Sent: 10 January 2012 08:52
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux?

Dave,

Sorry, but couldn't translate your response.

Was going to suggest to Gary that lead form damage to the lamps glass seal would be a primary candidate for early lamp failure as someone had suggested earlier.  All it takes is a bit of oxygen to slip in.

Can the observed difference in failure rates between RMA and the water soluble be that residual water soluble flux has eaten away at the Dumet lead at the glass to metal seal?  Dumet, being ~42Ni/58Fe 'rusts' with little additional assistance from acidic residues.

Steve C

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Monday, January 09, 2012 10:54 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning water soluble flux?


‰?z{S­©?}ê????xj??à*'µé?O*^µ?m?™Z?w!j»´
??³]é!?)??€´????…¸…????•??•…????”?µ½¹?½?µ½???”¥¸„??ˆ)?¥¹?„5•?±???????…•¹€?‘¥¥?…?????‰……¹”¸Q???½?‘?”?¼€‘¼?¼µ???”?•??????½??±±??¹??¥¥‘??½±½??¸Q??%
´??€)?…‘…??¥????”???½½°™½??”??½•‘?”?]??”?…???•????€???½½°???•?™±±?™??…¹??…???½‘?¥œ?…?????”?¸???)?½‘??½¸™…¥±?¥??¸??‘¥±?‰?¥¸????±?±?”?¼?…”€?‘?¥€)•¹¥??¥??½??????¬‰???…?¥???…±…??……¥…‰”???½µ±••±€)•?????()¸????……??¹?”´€????•…¥¹?‘‰…”??½±‘??‰”…‰??¥????”¥?)??•?±™?½¸„??„…™•?‰±?¥œ???™???Q???…???????…”€‘•…¥•???”?•…?¥???¥??…??½?…¥¹?•?…”?•™?¥??”?…µ¹…”??€????±‘?µ?¬…™•???????…?????±•¹¥œ?½±?¥¸?…?‰•¸?•µ?•¸€Q??”¥?…¸¥µ•¹”?µ½¹?½???±¥?•?‘?„½¸????‰©???¼???”¥?¹¼)¹•??¼???…½?•??•?¸)?”!¥±µ¸)½??•°?½±¥¹)‘?¥±µ??­•±?½±¥?¹½´(()½?”-½€?­½I4¹=4€)•¹?‰è?•?9•€?•?9•¥Œ¹?œ(?¼?¼???????4A±…?????¹??¼Q•?9??µ5¥°½?´?Q??•?%A¹=??A•…”?•?½¹??))???-¼€©­½%4
=?()Q(?•?9•%

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2