HI
Along time ago when I was involved with Ablefilm, you could option the glass
mesh thickness, [relative thickness to overall thickness], and on some
products the weave. This would - if you still can - give you the ability to
restrict the ooze also.
Regards
Mike Fenner
Bonding Services & Products
T: +44 [0] 1865 522 663 E: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Hernefjord
Sent: Tuesday, January 24, 2012 10:40 PM
To: [log in to unmask]
Subject: Re: [TN] Heatsink Bonding
William,
it seems to me as a question of viscosity. Ask for a film with somewhat
higher value or lower the processing temperature. The later will result in
longer processing time, which you may not accept if it's a high volume
line. We have been bonding boards on aluminum heatsinks for years with
Staystik 811 without flowing issues. Just as an example.
Inge
On 24 January 2012 16:18, William Noel <[log in to unmask]> wrote:
> Hello all - We have a project for which every PCB assembly needs to be
> bonded to a heatsink for thermal transfer from the devices on the board to
> the heatsink and out through the Heatsink mounting hardware to the box
that
> houses the assembled board/heatsink "modules". One of the requirements we
> have is that when the board assembly is mounted to the heatsink it needs
to
> be electrically isolated from the ground potential associated with the
> heatsink and box mounting hardware. As a result, we have used a
> combination of ablefilm and glass microspheres at the bonding interface
> between the board assembly and heatsink. The ablefilm serves as the bond
> and the glass microspheres provide electrical isolation. The problem we
> have consistently had with this process is squeeze out of the ablefilm
> through the holes in the vias of the board. We have attempted to use
> soldermask to tent the vias and thereby essentially seal the top surface
of
> the board. This has worked somewhat but we still seem to have problems
> with this approach. Does anyone else out there have experience with this
> and could share some advice with us. Thanks in advance for any help you
> can share.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask]
847-615-7100
> ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|