TECHNET Archives

December 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Eric Laroche <[log in to unmask]>
Date:
Tue, 13 Dec 2011 21:14:20 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Message-ID:
Content-Transfer-Encoding:
7bit
Subject:
From:
Bev Christian <[log in to unmask]>
X-cc:
Bev Christian <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (80 lines)
Eric,
You get what you pay for.  

Ideally you would affix strain gauges to your circuit packs, AFTER reflow
and follow the process.  Proper equipment to gather the strain gauge data is
a tad more expensive than 10 cross-sections, but once you have the
equipment, you can use it again and again.

When I am at work tomorrow I will send you the name of the equipment we use
- and like.

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric Laroche
Sent: Tuesday, December 13, 2011 8:36 PM
To: [log in to unmask]
Subject: [TN] cracked capacitors

Hi all,

We've been witnessing some field failures related to cracked 
capacitors.  We have seen it on different PCBA's, different panel 
configurations, different physical locations on boards even 3 different 
capacitor suppliers.  The only constant is that we always see it on the 
0,1uF ceramic 0603.  We've only had a couple of cross sections done as 
they are relatively expensive.  All cross sections done so far show 
evidence of board flexing causing 45degree cracks.

There must be something along our process that causes this flexing.  The 
way I see it, pretty much every step can be the guilty one.  From PnP, 
reflow, repair, ICT, functional testing, depanelling and final 
mechanical assembly...up to some extent, they could all possibly be 
causing flexing and damage to capacitors.  I would like to make a more 
extensive study to isolate the source of our problems.  Are there other 
methods, less expensive than cross sectioning, to see if a capacitor is 
cracked?

Have any of you faced this problem in the past?  What methods did you 
use to isolate the source of the problem?  What were your results?

Thanks for your help,

Eric

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2