Eric, You get what you pay for. Ideally you would affix strain gauges to your circuit packs, AFTER reflow and follow the process. Proper equipment to gather the strain gauge data is a tad more expensive than 10 cross-sections, but once you have the equipment, you can use it again and again. When I am at work tomorrow I will send you the name of the equipment we use - and like. Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric Laroche Sent: Tuesday, December 13, 2011 8:36 PM To: [log in to unmask] Subject: [TN] cracked capacitors Hi all, We've been witnessing some field failures related to cracked capacitors. We have seen it on different PCBA's, different panel configurations, different physical locations on boards even 3 different capacitor suppliers. The only constant is that we always see it on the 0,1uF ceramic 0603. We've only had a couple of cross sections done as they are relatively expensive. All cross sections done so far show evidence of board flexing causing 45degree cracks. There must be something along our process that causes this flexing. The way I see it, pretty much every step can be the guilty one. From PnP, reflow, repair, ICT, functional testing, depanelling and final mechanical assembly...up to some extent, they could all possibly be causing flexing and damage to capacitors. I would like to make a more extensive study to isolate the source of our problems. Are there other methods, less expensive than cross sectioning, to see if a capacitor is cracked? Have any of you faced this problem in the past? What methods did you use to isolate the source of the problem? What were your results? Thanks for your help, Eric ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 16.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------