I'm with Steve on this one...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, June 09, 2011 6:59 AM
To: [log in to unmask]
Subject: Re: [TN] Black Pad?
Hi Gary,
I got your pictures this morning, and have them posted now:
http://stevezeva.homestead.com/Joint_1.JPG
http://stevezeva.homestead.com/Joint_2.JPG
http://stevezeva.homestead.com/via.JPG
Although the pictures show some non-wetting happening, it's difficult to see
what exactly is going on.
You say that the component side seems fine, it's just when you're trying to
wave solder is when you see the problem. Maybe you have thin gold, and when
the boards were fresh, the SMT was able to solder fine. But then after the
boards went through reflow, the underlying nickel oxidized so badly that
solder wasn't able to wet?
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Robinson
Sent: Wednesday, June 08, 2011 4:46 PM
To: [log in to unmask]
Subject: [TN] Black Pad?
We have noticed a problem only on ENIG boards in our WAVE process that looks
similar to Black Pad but do not know how to identify or where to begin to
find a resolution to the problem. We were hoping an expert may have
experience in seeing this problem. Here are some facts -
1. Black residue is on the vias and thts on the solder side. Please see the
attached images.
2. Component Side SMT Parts do not exhibit the same problems.
3. Boards are processed PbFree - SAC305, Pacific 2009m No Clean Water Based
flux
4. THTs will not wet after residues appear (for touch up process)
5. Blowholes appear to accompany the defect but are not always present.
Thanks for your help in advance.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|