Paper/cardboard (unplasticised) is made from cellulose which is
hygroscopic. The absorbed humidity is sufficient to prevent static
charges from forming under all normal conditions; in fact, you would
have to work really hard to give it a charge even in low relative
humidity conditions. When I was a kid, we cut strips of kraft paper,
about 8 cm wide, held them in front of an electric radiant heater for
about 10 minutes (I guess they reached about 100°C), rubbed them like
hell on a trouser leg, and made some tissue paper figurines dance up to
them. The effect lasted no longer than five minutes without re-heating
the paper to dry it out again.
Brian
On 28/06/2011 22:15, Juan T. Marugán wrote:
> Hello all.
>
> There are some cardboard boxes (brown color) with the ESD symbol printed in the outer surface. I suppose the symbol only indicates that there is an ESD product inside, but I’m not sure. Am I right?
>
> Reason of my confusion: I’ve measured the surface resistance in these boxes and is 1x10E10 ohms: Static dissipative?...
>
> My concern is because de presence of these materials in the workshop. Mechanical parts, for example, are packaged in cardboard boxes and it is a hard work to re-package them into conductive boxes (plastic or cardboard) before to use them in the line.
>
> If somebody can give some idea, I’d appreciate it.
>
> Thank you so much.
>
> Juan
> Indra Sistemas. Spain.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|