Please see IPC-A-600 2.7.3 and IPC-TM-650 METHOD 2.4.1。
发件人: TGAsia [mailto:[log in to unmask]] 代表 Scott Li
发送时间: 2011年6月16日 12:00
收件人: TGAsia
主题: [TGAsia] Regarding Golden finger peel off
Hello All,
Our production line is encountering golden finger coating de-lamination issue when we perform the pull test between FPC and ACF.
Is there anybody has the standard which states the minimum bearing force for golden finger coating peel off.
Thanks,
Scott
Flextronics Tech(Shenzhen) Co.,Ltd
Tel No.:(86)755 89476888 Ext:8447
Address: Floor3, Block2, Yusheng Industrial Zone,XiXiang Section476(Gushu Roadside) Shezhen China.
Postal Code:518126 Emai: [log in to unmask]<mailto:[log in to unmask]>
Creating Value that increases Customer Competitiveness
Legal Disclaimer: The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
|
|
|