There are some cardboard boxes (brown color) with the ESD symbol printed in the outer surface. I suppose the symbol only indicates that there is an ESD product inside, but I’m not sure. Am I right?
Reason of my confusion: I’ve measured the surface resistance in these boxes and is 1x10E10 ohms: Static dissipative?...
My concern is because de presence of these materials in the workshop. Mechanical parts, for example, are packaged in cardboard boxes and it is a hard work to re-package them into conductive boxes (plastic or cardboard) before to use them in the line.
If somebody can give some idea, I’d appreciate it.
Thank you so much.
Juan
Indra Sistemas. Spain.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|