TECHNET Archives

April 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 5 Apr 2011 12:40:30 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Karen Tellefsen <[log in to unmask]>
Subject:
From:
Karen Tellefsen <[log in to unmask]>
Message-ID:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (79 lines)
A electoplating bath is necessarily conductive. The resistivity of the
water is not important, HOWEVER certain impurities will spoil.a plating
bath.

Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069



                                                                            
                                                                            
                                                                            
   [TechNet] DI water and plating                                           
                                                                            
                                                                            
   Douglas Pauls                                                            
                 to:                                                        
                    TechNet                                                 
                                                                 04/05/2011 
                                                                   12:03 PM 
                                                                            
                                                                            
                                                                            
                                                                            
   Sent by:                                                                 
          TechNet <[log in to unmask]>                                         
   Please respond to TechNet E-Mail Forum, dopauls                          
                                                                            
                                                                            
                                                                            






Good morning all.  I have a general question for those of you who deal
with electroplating.  How critical is the resistivity of the water to the
plating process?  I am not talking about impurities in the water, only the
resistivity of it?

Doug Pauls

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2