I'm not sure what your searching for but I'll share something about DI water and very thin or poor plating on products like the EMI shielding on certain connectors like for RJ45's. The shiny surface turned grayish or had water stain effects after cleaning in DI water.
The DI water wasn't the problem and the appearance was was strickly cosmetic however poor plating and a picky customer may have you polishing connectors.
I've only seen this happen a couple times over many years at a couple different companies, so I'm pretty sure our vendor engineers worked the issue with the vendors because the issue disappeared the next time we ran.
John Goulet
MFG/Process Engineer
----- Original Message -----
From: "Douglas Pauls" <[log in to unmask]>
To: [log in to unmask]
Sent: Tuesday, April 5, 2011 11:48:53 AM
Subject: [TechNet] DI water and plating
Good morning all. I have a general question for those of you who deal
with electroplating. How critical is the resistivity of the water to the
plating process? I am not talking about impurities in the water, only the
resistivity of it?
Doug Pauls
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|